Wire Cut EDM Parts

JR-3C Ointment Gel for HS-WEDM (Super Concentration)

JR-3C Ointment Gel for HS-WEDM (Super Concentration) or JR-3C EDM gel has high concentration, environmental friendly character, fast processing speed, good finish and good chip removal,...
Applicable to: TAGUTI EDM Type: HS-EDM PARTS SKU: Bottle
Size
Transport

$16.50

JR-3C Ointment Gel for HS-WEDM (Super Concentration) or JR-3C EDM gel has high concentration, environmental friendly character, fast processing speed, good finish and good chip removal, suitable for processing large thickness workpieces.

JR-3C Ointment Gel for HS-WEDM (Super Concentration)

◆ Concentration Solution:

- Put the ointment into running water with a ratio 1:70-80 and stir until mix the ointment into water thoroughly;

- Avoid hard water such as well water or ground water.

◆ Ingredients: Green product for the environment

◆ Using range: It is used for cooling of wire electric discharge cutting of various metal materials (HS-WEDM) and also suitable for cooling of metal cutting.

◆ Features: The product is improved based on JR-3A gel, which inherits all the advantages of JR-3A.

  1. The productJR-3C is currently the highest concentration of working liquid;

  2. Uniform and whitefinish surface without commutation stripes after the workpiece is cleaned with kerosene;

  3. Under high-energy processing conditions (average processing current>5A), it has good cutting stability. Compared with traditional emulsified oil, JR-3C’scutting efficiency is increased by 30%, the surface quality is improved by half, the electrode wire loss is reduced by 50%, and the service life of molybdenum wire greatly extended;

  4. There is basically no foam during processing, and workbench surfaceis clean;

  5. Suitable for cutting within 500mm thickness die steel.

Specially suitable for multiple-cut of WEDM-HS.

◆ Expire Date:12 months

◆ Package: 2KG Special Plastic Bottle. 18KG / BOX, (2*9 bottles)

◆ Attention:

  1. When replenishing, please add JR-3Cand water in proportion;

  2. Please use themagnet to suck the workpiece after cutting, so as not to drop and break the molybdenum wire;

  3. When cutting large thickness, properly slow down the variable frequency tracking speed, adjusting from zero to stable cutting, and the ammeter will basically no longer shake.